Veröffentlichungen
Simulation of the Microstructure Evolution during Directional Solidification and Solution Heat Treatment of Superalloys
- Authors
N. Warnken, D. Ma, A. Drevermann, I. Steinbach and S. G. Fries
- 2007
- Journal Article
Journal:
Transactions of the Indian Institute of Metals
Volume:
60
Issue:
2-Mar
Pages:
293-297